AQUAPOXY
Two components water-based epoxy primer
CAT. NO. : 425A, 425B
Aquapoxy is Environmentally friendly, low odor, does not contain any solvents.
Aquapoxy has good chemical resistance, excellent durability, and excellent adhesion properties for polyurethane and acrylic systems.
Aquapoxy is used as a primer for Multigum, G18, Polyseal and Aquatec prior to application on concrete, bitumen membranes coated with aggregates, old acrylic and polyurethane coatings
Product description |
Aquapoxy is Environmentally friendly, low odor, does not contain any solvents. Aquapoxy has good chemical resistance, excellent durability, and excellent adhesion properties for polyurethane and acrylic systems. |
Application | Aquapoxy is used as a primer for Multigum, G18, Polyseal and Aquatec prior to application on concrete, bitumen membranes coated with aggregates, old acrylic and polyurethane coatings. |
Technical data | Solids content (by weight) 55%
Specific gravity approx. 1.1 Viscosity, pa s 1 Mixing ratio A=7.6 ; B=3.7 Pot life after mixing (at 25ºc) 45 – 60 minutes Dilution & cleaning water |
Surface preparation | The surface will be clean, dry and stable, without loose particles. In case of concrete, the surface will be washed with high pressure water jet (500 bar or by sand blasting), to remove the surface cement skin and expose concrete holes.
Afterwards, the surfaces will be treated according to the instructions of the designated coating. |
Preparation of the product | Pure Aquapoxy part B (3.70 kg) into Aquapoxy part A (7.60 kg), then add water up to 3 cm under pail upper edge, mix slowly (100-200 rpm) the two components by electric drill mixer for 3-5 minutes to obtain homogeneous material and let it rest for 10-20 minutes prior to coating. |
Instruction for use | Aquapoxy may be applied by brush, roller or airless spray. Surface preparations and other application details will be according the instructions of the designated coating. when using airless, cleaning of machine will be done with toluen. |
Drying time | Drying time prior to application of next layers: 1-2 hours (at 25ºc and 50% RH).
In summer period, drying time will be 1 hour in general. In winter time, drying time will prolong to 4 to 5 hours. In any case, the next layer should be applied on tacky Aquapoxy layer, and not on dry glossy material. |
Consumption | 250 gm/m² on concrete and old bitumen membranes covered by aggregates.150 – 200 gm/m² on old acrylic and polyurethane coating. |
Storage | In a shade, protected against frost and high temperatures (5ºc - 35ºc) |
Packaging | Part A – 7.60 KG
Part B – 3.70 KG Total net weight after adding the water due to instructions – 18 kg. |
Warning and safety measures |
|